How do you when Albrite that you are using has lost its ability to cleanup/etch into your species?. Also does putting it into the sun (warmth) help the cleanup process?

Rob P.


My Avatar is my kind of gold -- SDC 2300, Xterra 705, GPZ 7000

#2

mbasko
Member
From: Central West NSW
Joined: 27 January 2015
Posts: 2,728
Member
22 December 2016 02:58 pm

You should be replacing the Alibrite periodically i.e. dispose of old solution once a week or so & refill with fresh solution. I always pour the old solution thru a stainless steel tea strainer in case any golds broken away.
I don't believe heating it up will help the process any. Alibrite is a slow method. A dolly pot is quicker but doesn't leave your gold looking as nice lol

Last edited by mbasko (22 December 2016 02:59 pm)


Everything we use comes from mining or farming.

1 user likes this post: PabloP

#3

PabloP
Member
From: Melbourne or travelling
Joined: 18 January 2015
Posts: 652
Member
22 December 2016 03:56 pm

Thanks. Definitely slows down the process after a week or so. I am more interested in having the small wire gold stand out a bit more so not interested in smashing them.

Rob P.


My Avatar is my kind of gold -- SDC 2300, Xterra 705, GPZ 7000

#4

BigWave
Member
From: Melbourne
Joined: 19 January 2016
Posts: 1,840
Member
22 December 2016 04:25 pm

Don't forget here's only around 5% HF in Ali Brite, so it doesn't take much reaction with ironstone to significantly use up the acid. In the bottle it should have very long life